b'STAGE3 Lamination Process - Skin CoatApplying SkinApply the Skin Coat SKINCOAT - Using R6800 TPA Coat ResinResin 6800PA pre vinylester resin with tissue and 6800PA 300CSM allow to cure for 23 hours.A skin coat gives benefits of improved surface aspect reduced print through of reinforcement and it can better resist the effects of fatigue which can cause cracking in hard-worked structures such as moulds. Vinyl ester can also withstand temperatures of up to around 200 0 C without distorting.Vinyl EsterImportant if post curing! Tooling Gelcoat GC 206/207PAPolished,Sealed and Waxed PlugApplying Tooling Resin Norester RM 2550 or RM 3000Apply the Skin Coat Mould thickness is dictated Resin 6800PA by thickness of part being manufactured, normal Apply Toolingrequirement is 3:1 in ratioResin Norester Resin RM 2550(e.g. if you are making a 3mm part, your or Resin RMmould thickness will need to be 9mm)3000Follow TDS for amounts Vinyl Ester Polished, required for this processTooling GelcoatSealed and GC 206/207PA Waxed PlugBULK LAYERS WITH NORD 2000/50 TOOLING RESINWhen using the resin system, it is extremely importrant to mix throughly before using and also get theCured back face of mouldtemperature between the required specifications. (if used at temperatures too cold you will not achieve the required exothermic reaction).'